Abstract
Hexagonal prism-like ZnO crystals dominated with polar facets were synthesized using a hydrothermal method. The Gold (Au) nanoparticles were selectively photodeposited on the polar surfaces of faceted ZnO crystals as a result of anisotropic photocatalytic activities of the polar and nonpolar facets. The size of Au nanoparticles uniformly dispersed on the polar facets increased with increasing Au-loading amount. These Au-loaded ZnO crystals showed an additional visible light absorption band from 400nm to 800nm. The 0.1wt% Au-loaded ZnO crystals with visible light absorption peak at approximately 690nm exhibited the highest photocatalytic activity under visible light irradiation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.