Abstract
In order to obtain fine mullite powders by a simple and inexpensive process, alpha aluminum hydroxide (α-Al(OH) 3) was used as raw material, and heterogeneous nucleation-and-growth process was chosen for the preparation of powders. Composite coating particles consisting of α-Al(OH) 3 cores with outer amorphous silica shell were prepared by heterogeneous nucleation-and-growth process in the ethanol suspension containing ammonia, tetraethylorthosilicate (TEOS) and α-Al(OH) 3. Fine mullite powders (average particle size 0.67 μm) were fabricated by calcined composite coating particles at 1500 °C for 2 h.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.