Abstract
We present the fabrication of large format $640\times512$ , 15- ${\mu }\text{m}$ pitch, mid-wave infrared region (MWIR) InAs/GaSb type-II superlattice (T2SL) focal plane array (FPA). In this report, the details of device design and fabrication processes are withheld adhering to the common practice of most of the manufactures and developers because of the strategic importance; however, information about fabrication processes of T2SLs FPA is presented to a certain extent. Comparison of etching techniques, passivation materials and methods, and substrate thinning (mechanical and chemical) is given besides of details regarding the standard ohmic contact and indium (In) bump formations. Morphological investigations of fabrication step are included. Large area pixels, $220\,\,{\mu }\text{m}\,\,\times 220\,\,{\mu }\text{m}$ , fabricated by different etching methods and passivation materials/methods are compared in terms of dark current levels. Wet passivation with (NH4)2S is discussed in terms of morphological investigations, and dark current results are compared with untreated samples. Large area pixel level characterizations as well as image level benchmarking of mechanical and chemical substrate thinning are reported. Effect of GaSb substrate on device performance and the way of reducing stress of In bumps are revealed. The importance of complete substrate removal is demonstrated through FPA images.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.