Abstract

Explosive consolidation of Sm 2 Fe 17 N x and Sm 2 Fe 17 N x /(Ni or Co) magnetic powders were attempted to consolidate fully dense magnetic compacts. Dense Sm 2 Fe 17 N x and Sm 2 Fe 17 N x /(Ni or Co) bulk materials were obtained by cylindrical explosive consolidation technique using water as a pressure transmitting medium. The values of ( BH ) max of Sm 2 Fe 17 N x , Sm 2 Fe 17 N x –5 wt%Ni and Sm 2 Fe 17 N x –30 wt%Co magnets obtained were 23.8, 16.3 and 17.5 MGOe (190, 130 and 140 kJ / m 3 ) , respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.