Abstract

The induction heating of the billets is a critical step in the thixoforming process. To improve the quality of thixoforming, the induction heating strategy should be investigated. In this study, by using an induction heating system of 50 kHz, multi-step reheating schemes were adopted to reheat the nondendritic A356 alloy to the temperature between the solidus and liquidus line. To obtain uniform temperature distribution and fine globular microstructure, the effects of the reheating parameters, such as reheating time, reheating temperature, holding time and holding temperature, were investigated. Then the analysis of the final temperature difference and the optical microstructure of the reheated billets were conducted, the results showed that two-step reheating process is suitable for A356 alloy with the size of 45 mm × 25 mm, and the suitable time for the final holding process is 2 min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.