Abstract

The mortar board was prepared with the content of reduced iron powder, thickness and shielding fabric as variables. The results showed that appropriate content of reduced iron powder could improve the shielding efficiency of mortar, and the peak shielding efficiency of 10mm thick specimens with a dosage of 300kg/m3 reached 16.9db and the 20mm-thick specimens reached 17.1db. The 10mm-thick specimens with shielding fabric reached 73.5db, and the 20mm-thick specimens reached 59.3db

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.