Cylindrical lab-scale tank based on 98.0g of the Mg(NH2)2–2LiH–0.07KOH compacts was designed. Hydrogen storage properties of the tank, including bed temperature, hydrogen pressure and flow rate in the hydrogen absorption and desorption process were investigated under a variety of conditions. In the hydrogen absorption process of which the applied hydrogen pressure is 6.0MPa, the central temperature of the hydride bed increases obviously from 453K to 524K. Furthermore, the increase of the applied hydrogen pressure can lead to greater changes in the bed temperature. The hydrogen desorption process exhibits 3 stages under the constant flow rate mode, and the hydrogen desorption of Mg(NH2)2–2LiH–0.07KOH mainly carries out at stage II accompanied with a significant temperature drop. As the flow rate increases, the endothermic dehydrogenation of the hydride degrades the bed temperature to a lower value, and the amount of hydrogen released also decreases at this stage. The results indicate that an efficient improvement of the heat transfer property for the Li–Mg–N–H based tank is needed to improve its sorption behavior.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.