In order to reduce the volume fraction of H2S in the water wall area of the four-corner tangential boiler and achieve the purpose of alleviating the high temperature corrosion of the water wall, a thorough test was carried out on the 600MW boiler. The results show that the high temperature corrosion of the water wall under high load is obviously more serious than that under low load, the high temperature corrosion of the water wall of the front wall is more serious than that of the other walls, and the high temperature corrosion of the furnace wall area downstream of the burner is generally higher than that of the other walls. Other areas. The reason for this phenomenon is that the uniformity of the pulverized coal quantity in each pulverized tube is large, the air distribution is unreasonable, the primary and secondary air are separated, and the secondary air cannot completely cover the primary air; The uniformity of pulverized coal distribution, the proper increase of the total air volume, and the proper increase of the perimeter air volume can significantly reduce the volume fraction of H2S in the water wall area and alleviate high temperature corrosion.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.