Abstract

A certain multi-metallic lead-zinc oxide ore contains 1.09%Pb,8.39%Zn. The oxide rate of lead and zinc is 96.34% and 98.15% respectively.In order to recover valuable minerals from the oxide ore comprehensively, the authors adopted priority flotation processing in this experimental research. At last, the lead concentrate with Pb grade of 27.41% and the zinc concentrate with Zn grade of 24.14 % were respectively achieved. The overall recovery of lead was 93.66%,and the overall recovery of zinc was 90.74%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.