In this paper, the experimental behaviour of mud brick reinforcement is present. The effect of natural fibers such as straw, wood chips carpentry, rice husk and palm fibres on the compressive strength, Young’s modulus, proper durability against water and tensile strength of brick samples were given. Different amount of fibres were selected to test: 0.3 and 0.6 and 0.9 percentages of specimens’ weight. The amounts of each component which may be effect the mechanical behaviour of mud bricks were investigated. In accordance with the results, the best sample in terms of compressive strength and durability against water is determined.In this investigation, the compressive strength and tensile strength of mud brick is studied. For the compressive strength the cubic samples with dimensions of 22×22×7cm and 22×11×7cm, and for the tensile strength the cylindrical samples with a diameter of 15cm and height 30cm were tested. The compressive strength of simple sample mud brick is 4.4MPa. The compressive strength of the samples with natural additive is between 2.67 and 16.53MPa. The durability against water of simple specimen is 255min and the sample with 0.9 percent of weigh rice husk is 560min. The natural additives increase the tensile strength from 57 to 281 percent.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.