Abstract

Hybrid metal matrix composites are being widely investigated for use in light weight, high strength applications. In the present study, Aluminium alloy Al7075 was reinforced with B4C and TiO2at 4% and 2% weight fractions respectively. The powders of the reinforcements were ball milled for uniform distribution in the Al matrix, and later fabricated by stir casting technique primarily due to simplicity and economy of the method. The specimen were prepared as per ASTM standards and later subjected to hardness, double shear, wear and impact tests and the results were compared with that of pure aluminium specimen fabricated by the same method. The hardness, shear strength, impact strength of the composite were found to be higher than pure aluminium by 4.97%, 32.28% ands 6.41% respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.