Abstract

A mechanism of thermocracking, which occurs in an alumina ceramic ring of a mechanical face seal, is proposed based on experimental and analytical results. Methods for its prevention are also discussed. The experiments were conducted using an external type mechanical face seal composed of a carbon ring and three kinds of alumina ceramic rings, with distilled water as the liquid to be sealed. By using a layer of gold vacuum deposited onto the surface of the ceramic ring as a part of a DC circuit, the moment of crack initiation was identified. The thermal stresses produced in the ceramic ring by frictional heating were calculated using finite element analysis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.