Static experiments have been developped to investigate the R7T7 glass corrosion in four natural salt brines (brines 1 and 3: pure halite, brines 2 and 4: high Mg, K fluid inclusions rich halite), at 90°C and 150°C with 0.7 cm −1 S/V ratio and at 11 different running times. Analysis of brines after alteration (pHmeter and ICP) added to a detailed study of the crystalline phases developped at the interface glass-brine (XRD, SEM and Microprobe), showed that the influence of the compositional difference is more important on the nature of the secondary phases formed than on the corrosion rate of the glass. After 91 days of alteration at 150°C stady states seems to be reached (after 40 days at 90°C).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.