AbstractThe major adhesive resin worldwide used in the manufacture of plywood is phenol formaldehyde resole (PF) resin. The raw material for this kind of adhesive is derived from petroleum oil. Because of rising prices of crude oil and the scarcity of petroleum products, their replacement by natural resource–based raw material has become a necessity. In the present work, the possibility of replacing phenol in PF resin with lignin was explored. The parameters for preparation of bark lignin substituted PF (LPF) adhesive, such as lignin concentration, formaldehyde to phenol molar ratio, catalyst concentration, reaction time, and reaction temperature, were optimized. It was found that up to 50 wt % of phenol can be substituted by lignin to give an LPF adhesive with better bonding strength compared to that of control PF resin. Prepared resins were characterized using IR, DSC, and TGA. IR spectra of LPF adhesive showed structural similarity with that of PF adhesives. Thermal stability of LPF adhesive was found to be lower compared to that of control PF (CPF) adhesive. DSC studies revealed a lower curing temperature for LPF resin than that for CPF resin. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 3514–3523, 2004

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.