Abstract
The correct address for Materials Science, University of Texas at El Paso is 500 W. University Avenue, El Paso, TX 79968, USA. As specified in the original article, the data for UTS, elongation to break and Young’s modulus for the ABS loaded with TiO2, jute fiber and TP elastomer were based on three specimens instead of five specimens. Tables 3 and 4 are updated with the correct data. The data for ABS remains the same. Table 3 Values of UTS and UFS for XYZ specimens
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.