Abstract
REE-Nb-Fe ore is a typical refractory resource rich in valuable elements. In this article, coal-based reductive roasting followed by magnetic separation is proposed to recover rare earth element (REE), niobium (Nb), and powdered metallic iron (Fe) concentrate from a REE-Nb-Fe raw concentrate containing 31.9% total iron grade (TFe), 3.2% rare earth oxides (REO), and 2.9% Nb2O5. Sodium sulfate is employed to enhance the reduction of iron oxide and to facilitate the growth of metallic iron grains. A magnetic fraction with TFe of 89.3%, iron metallization of 95.8% and iron recovery of 91.5% is obtained by magnetic separation after the raw concentrate is reduced to 1100°C for 120 min in the presence of 15 wt.% sodium sulfate. The contents of rare earth and niobium in the nonmagnetic fraction are enriched to 5.4% (REO) and 4.6% (Nb2O5) with recoveries of 96.1% and 95.8%, respectively. The TFe in the nonmagnetic fraction obtained after the separation is decreased to 4.8% accordingly. The reactions between sodium sulfate and SiO2/Al2O3 enhance the reduction by destroying the mineral structure. The separation of iron from rare earth and niobium is highly improved as metallic iron grains grow markedly when roasted in the presence of sodium sulfate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.