Abstract

ABSTRACTAcrylonitrile–butadiene rubber (NBR) with different acrylonitrile (ACN) contents was filled with barium titanate (BT) to prepare the polymer dielectrics. The neat NBR, NBR/untreated BT, and NBR/bis‐(γ‐triethoxysilylpropyl)‐tetrasulfide (silane coupling agent KH845‐4) modified BT (MBT) composites were prepared. At low ACN content (ACN content 20 wt %), the tensile strength of the NBR/MBT composites increased by 173.6% from 2.69 to 7.36 MPa compared to the neat NBR. The pleasing results were not found in those composites with high ACN content. Both surface modifications of BT and NBR with low ACN content would result in lower interfacial tension between BT and NBR. A strong interfacial adhesion was observed between MBT and NBR with 20 wt % ACN content. The interfacial adhesion had great contribution to the mechanical strength of composites. Moreover, the dielectric properties of composites were also investigated in detail. The addition of BT enhanced the dielectric constant of composites markedly. This study can be applied in manufacturing electronic devices, which are subjected to oily environments for a long time. At the same time, the study can provide some help for researchers to select the polymer matrix and the appropriate surface modification agent of functional filler. © 2017 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018, 135, 45936.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.