Abstract
Abstract The influence of several additives (ZrO 2 , CeO 2 , TiO 2 , SiO 2 ) on sintering of conventional yttria powders is investigated. Titanium oxide is the most efficient in promoting densification and in lowering sintering temperatures. Almost full densities can be obtained at 1400–1500°C if a small amount of dopant (0.2 wt% TiO 2 ) is dispersed homogeneously onto the surface of yttria during powder processing.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.