Wollastonite and porcelain–wollastonite coatings on stainless steel were obtained by electrophoretic deposition using acetone as dispersive medium. A direct electric current of 800 V for 3 min was used for obtaining the single wollastonite coating. A well-sintered layer was observed after heat treatment at 1050 °C for 1 h in air. The two-layer coating was obtained by depositing dental porcelain at 400 V for 30 s followed by the deposition of wollastonite at 400 V for 3 min. After forming the two layers, this complex coating was heat treated at 800 °C for 5 min. Under these conditions, strong bonds of both the interface wollastonite–porcelain and that of porcelain–metallic substrate were observed. The in vitro bioactivity assessment of the coatings was performed by immersing the deposited substrates in simulated body fluid (SBF) for 21 days. All the materials showed to be highly bioactive through the formation of a homogeneous apatite layer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.