Abstract
Electronic functionalization of complex fiber systems is important for new applications in energy systems and electronic textiles. The cover image shows a natural fibrous material with and without conductive coating. Atomic layer deposition (ALD) of conductive coatings on natural and synthetic fibrous materials show high conductivity, and the values scale as expected with film thickness and bulk-material conductance. On page 1993, Jesse S. Jur and co-workers present an all-fiber-based capacitor formed by ALD on textiles that shows good sensing performance in several liquid media.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.