The dense surface passivation layer on zero-valent iron (ZVI) restricts its efficiency for water decontamination, causing a poor economy and waste of resources. Herein, we found that the ZVI on Fe-Mn biochar could afford a high electron-donating efficiency for the Cr(VI) reduction and immobilization. Over 78.0% of Fe in the Fe-Mn biochar was used for the Cr(VI) reduction and immobilization, i.e., 56.2 − 161.7 times higher than the commercial ZVI (0.5%) and modified ZVI (0.9 −1.3%), indicating that the unique ZVI species in Fe-Mn biochar offered an outstanding Fe utilization efficiency. We proposed that oxygen atoms in the FeO in the FeMnO2 precursor were removed during pyrolysis with biochar while the MnO skeleton was preserved, forming the embedded ZVI clusters within Fe-Mn oxide. The unique structure inhibited the formation of the Fe-Cr complex on Fe(0), which would facilitate the electron transfer between core Fe(0) and Cr(VI). Moreover, the surface FeMnO2 inhibited the diffusion of Fe and facilitated its affinity with pollutants, thus supporting higher efficiency for pollutant immobilization. The preserved performance of Fe-Mn biochar was proved in industrial wastewater and after long-term oxidation process, and the economic benefit was evaluated. This work provides a new approach for developing active ZVI-based materials with high Fe utilization efficiency and economics for water pollution control.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.