Abstract
This paper presents the results regarding the electrochemical stability and surface analysis of a new alkyd paint with low content of volatile organic compounds in comparison with a conventional alkyd paint. The alkyd films were realized on carbon steel substrate. Dry films thickness in 30–35 μm range was obtained. The experimental tests were carried out in 3% NaCl solution at the 25 °C temperature. The electrochemical techniques (electrochemical impedance spectroscopy (EIS), potentiodynamic and Tafel polarization) and surface analysis techniques (AFM, SEM, EDX) were used to evaluate protective properties of the tested paint films. The correlation of all experimental results established that the new alkyd paint with low content of volatile organic compounds presents better protective performances and lower permeability than conventional alkyd paint. AFM, SEM and EDX indicated a compact, homogenous, non-porous and adherent coating.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.