Abstract

Spherical porous Mn2O3 powders were prepared by spray pyrolysis. Li and Al nitrate solution were immersed to porous Mn2O3 powders to obtain LiAlXMn2-XO4. Homogeneous LiAlXMn2-XO4 powders were formed by the calcination at 800°C. SEM observation showed that they had spherical morphology with particle size of about 1m. XRD revealed that the spinel phase was obtained by heating at 800°C. LiAlXMn2-XO4 cathode obtained by this method exhibited higher rechargeable capacity and cycle stability than that obtained by spray pyrolysis. The doping of Al ion was effective for the cycle stability at elevated temperature.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.