Abstract

Increase in the wire axial deformation and the strength of joining welded wire to a component at the expense of the roller rotation retardation at the invariable values of the other welding conditions, specifically of the welding heating cycle force and duration, are shown and substantiated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.