Abstract

Abstract This study presents novel results from in-situ stress relaxation tests using rubber O-ring seals immersed in bio-lubricant base oils (jojoba, soybean and palm oil), with a mineral base oil used for comparison. Little information is available on the interaction of bi-lubricants and elastomers. The use of Hanson Solubility Parameter modelling methods was considered for assessing compatibility. Some correlation was found between experimental results for EPDM. Results were inconclusive for NBR and FKM. EPDM immersed in palm and soybean oil suffered minor shrinkage, caused by stress relaxation. Swelling occurred with EPDM immersed in jojoba and mineral base oil, caused by diffusion. Results for nitrile showed shrinkage for all oils. Less than 1% change in mass occurred for all oils and FKM.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.