Abstract

The porosity number and porosity area percentage of weld beads close to the weld surface reduce after ultrasonic peening treatment. The grains are refined significantly in severe deformation layer and transition layer. The refined grain size is approximately 200nm on the surface of weld bead after ultrasonic peening treatment. The loads on severe deformation layer and transition layer are larger than those on weld beads without ultrasonic peening treatment with the same indentation displacement in nano-indentation tests. After ultrasonic peening treatment, the elastic modulus of the weld bead surface increases slightly due to the decrease of porosity fraction. The hardness values of severe deformation layer and transition layer increase, which leads to the enhancement of wear resistance of welded joints.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.