Mg matrix composites with SiC particles ranging from 5vol%–25vol% were prepared using stirring casting method. Die casting, squeezing casting, and extrusion were applied for inhibiting or eliminating the defects such as gas porosity and shrinkage void. Through die casting and squeezing casting, most of the defects in Mg matrix composites could be eliminated, but the mechanical properties were improved limitedly. On the other hand, after hot extrusion, not only most of the defects of as-cast composites ingots were eliminated, but also the mechanical properties were improved markedly. With the addition of SiC, the tensile strength, yield strength and elastic modulus of as extrusion SiCp/AZ61 composites increased remarkably, and the elongation decreased obviously.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.