Abstract
The effects of heat treatment on the microstructure, residual stresses, nano-indentation behavior, the resistance to the corrosion and cavitation erosion (CE) of 17-4PH stainless steel (17-4PH SS) by laser surface melting (LSM) were thoroughly investigated. Experimental results showed that the samples were mainly composed of martensite phase, and the NbC precipitations formed after heat treatment. The distribution of NbC precipitations was more uniform in the sample (S3) after solution treatment 3 h at 1040 °C + aging treatment 3 h at 480 °C. The grain size was increased for the samples after heat treatment. This heat treatment processing significantly reduced the residual stresses generated from the LSM process, and the nano-indentation behavior of the LSM samples after heat treatment was improved compared to that of the LSM sample without heat treatment. The S3 sample displayed the highest corrosion resistance as indicated by the low corrosion current density (icorr), high pitting potential (Epit) and high polarization resistance (Rp). The CE resistance of samples after heat treatment in 3.5 wt% NaCl solution was higher than that of the sample without heat treatment. Among them, the S3 sample exhibited the highest CE resistance, and its CE mass loss was only 59.5 % of the sample without heat treatment. The excellent CE resistance resulted from the appropriate combination of mechanical properties, corrosion resistance and self-recovery ability of the passivation film.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.