Abstract

Background: Ceramic restorations are widely used nowadays as the esthetic demand has increased in the worldwide population, and lithium disilicate and feldspathic porcelain materials are the most widely used veneer materials. The traditional removal procedure for veneers was recently replaced with the use of laser technology to debond the veneers so that the de-bonded veneers can be preserved and re-used. Aim: Up to now, there have been few studies regarding using lasers to remove ceramic laminate; thus, it is clear why this research topic is important for examining the efficiency of lasers in the use of de-bonding for different ceramic laminates with varying compositions and materials. Materials and Methods: This study employed forty-five normal human maxillary first premolars with comparable proportions. The forty-five teeth were initially split into three groups of fifteen teeth, and the teeth were chosen at random. Each group fused pairs of various ceramic materials. A total of fifteen teeth in the first group underwent feldspathic porcelain restorations. The second group contained fifteen restorations made of lithium disilicate glass-ceramic CAD-CAM. In the third group, fifteen teeth were restored using glass-ceramic that had a lithium disilicate glass-ceramic ingot. The RelyX Veneer A1 shade, available from 3M EPSE in the United States, was used to bond all the samples. The specimens were then submerged for approximately 24 h in distilled water at 37 degrees Celsius in order to simulate the conditions in an oral cavity. An Er,Cr: YSGG laser (Waterlase, iPlus, Biolase, from USA) was used with a turbo headpiece and an MX7 sapphire tip for irradiation. Results: The time needed for the ceramic disc to debond was calculated using a digital stopwatch. The average removal times for the feldspathic porcelain, lithium disilicate glass-ceramic ingot, and lithium disilicate glass-ceramic CAD-CAM were 10.067 ± 1.668 s, 5.200 ± 1.146 s, and 5.133 ± 1.125 s, while the removal times ranged from 8–12 s, 4–7 s, and 4–7 s, respectively. Compared to the other ceramic materials, de-bonding the feldspathic porcelain took longer. Conclusions: According to this study, the Er,Cr: YSGG laser application using the same study parameters made it simpler to de-bond lithium disilicate and feldspathic porcelain. Lithium disilicate, as opposed to feldspathic porcelain, transmits laser light more effectively; hence, the results varied depending on the materials, and the debonding occurred primarily at the veneer–cement interface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.