Abstract

Solution chemical reduction method is a means which used reducing agent in aqueous or organic systems to deoxidize silver ions. Its essence is an integrated process of the electrochemistry, thermodynamics, kinetics and fluid dynamics and so on. The process determines the physical and chemical properties such as the size distribution of powder, purity and reunion situations, etc. Nano-silver powder has high surface activity and catalytic properties, and is widely used to a lot of fields. So it has very important realistic significance to study the preparation method. In this paper, nano-silver powder was prepared with industrial AgNO3 as raw materials, sodium borohydride or hydrazine hydrate as reducing agent, polyvinyl alcohol, SDBS or polyvinylpyrrolidone(PVP) as the surface protective agent by solution chemical reduction method. The influences of different reducing agents and protective agents on the preparation of nano-silver were analyzed. The results from the XRD diffraction analysis and TEM show that it can be obtained high purity flake nano-silver in the reaction temperature range of 50-60°C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.