AbstractThe potentiodynamic polarization test and slow strain rate tensile tests of X80 pipeline steel were performed in 0.5M Na2CO3-1M NaHCO3solution to study the electrochemical and stress corrosion cracking properties. The results of potentiodynamic polarization test show that there is an obvious stable passive region, about from 0v to 0.8V (SCE), indicating that anodic protection is feasible. The results of slow strain rate tensile tests show that the stress corrosion cracking sensibility is high and cathodic protection effect is restricted due to the hydrogen permeation. However, the elongation, yielding strength and tensile strength all increase with anodic protection. The higher anodic protection potential in the stable passive region is benefit to improve tensile strength and yielding strength. However, the higher elongation is obtained at 0.5V (SCE) anodic protection potential.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.