Abstract

In this study, the microstructural and densification behavior of titanium nitride (TiN) and titanium carbonitride (TiCN) reinforced Ti-6Al-4V were investigated under an applied pressure of 50 MPa, sintering temperatures of 1000–1100 °C, heating rate of 100 °C/min and dwell time of 10–20 min through spark plasma sintering technique. Results show that the microstructural transformation of the titanium matrix composite comprises of a mixture of lamellar colonies with β grain boundaries and nanoparticles with an average grain size range of 4.5–6.0 μm. Furthermore, an addition of nanoceramics TiN/TiCN resulted in microstructural transformation, uniform particle distribution within the metal matrix and along the grain boundary. However, the sintered relative density of the composites decreased with the percentage increase in TiCN, while fully dense composites were obtained at a sintering temperature of 1100 °C. Microhardness values of the sintered composites reach a greater level in comparison to Ti-6Al-4V alloy while fracture morphology of the sintered composites with addition of nanoceramics (TiN/TiCN) displayed a transgranular transformation within the matrix accompanied with fine dimple features.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.