The structure, phase composition and mechanical properties of (α+β) — titanium alloy solution treated at 850 °C, cold-rolled at the reduction ratio in the range of 0… 45%, followed by ageing at 450, 500, 550 °C for 0.5, 1.5, 3 hours was studied using XRD, microindentation and tensile testing. The influence of strain level at cold rolling and time-temperature parameters of ageing on the formation of structure and phase composition of solution treated and water quenched Ti-3Al-5Mo-4.5V alloy was investigated and discussed in terms of tensile properties and microhardness. The parameters of low temperature thermomechanical treatment (LTMT) of the (α+β) — alloy were proposed to obtain a high-strength state.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.