Abstract
The impact property is one of the most significant mechanical properties for metallic materials. In the current work, a soft–hard copper–brass block with a high yield strength of ~320 MPa and good uniform elongation of ~20% was prepared, and the effect of the testing temperature on its impact property was explored. The results showed that the impact energy was decreased with the increase in testing temperature. The impact energies at liquid nitrogen temperature (LNT), room temperature (RT), and 200 °C were 8.15 J, 7.39 J, and 7.04 J, respectively. The highest impact energy at LNT was attributed to the coordinated plastic deformation effects, which was indicated by the tiny dimples during the process of the delamination of soft–hard copper–brass interfaces. The high temperature of 200 °C can weaken the copper–brass interface and reduce the absorption of deformation energy, result in low impact energy.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.