Abstract
Nanocrystalline MgSnO 3 powders have been synthesized using co-precipitation method in presence of sodium bis(2-ethylhexylsulfosuccinate), Aerosol OT (AOT) as anionic surfactant. Statistical Box–Behnken experimental design was used to investigate the effect of main parameters (i.e. surfactant concentration, calcination time and calcination temperature) on MgSnO 3 powders formation, crystallite size, particle size mean diameter and morphology. MgSnO 3 particles were investigated using XRD, SEM, and laser diffraction particle size analysis (Coulter LS 13 320). XRD patterns revealed that the magnesium meta-stannate MgSnO 3 was single phase at 800 °C and the peaks intensities were changed by increasing the calcination temperature from 1000 to 1200 °C due to the decomposition of meta-magnesium stannate MgSnO 3 to ortho-magnesium stannate Mg 2SnO 4 and stannic oxide SnO 2. SEM micrographs showed that the morphologies of the powders formed were changed by increasing the calcination temperature from 800 to 1200 °C from foam-like structure to rectangular-plate shape. Coulter LS 13 320 showed that the average particle size diameter was about 4.43 μm. The results indicated that the calcination time, calcination temperature and surfactant addition were significant on the produced magnesium stannate mean diameter.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.