AbstractPoly lactic acid (PLA)/Banana fiber (BF) biocomposites were fabricated employing melt blending technique followed by compression molding. BF were surface‐treated by NaOH and various silanes viz. 3‐aminopropyltriethoxysilane (APS) and bis‐(3‐triethoxy silyl propyl) tetrasulfane (Si69) to improve the compatibility of the fibers within the matrix polymer. Mechanical tests revealed an increase of tensile strength to the tune 136% and impact strength to 49% as compared with the untreated biocomposite. Thermal properties of the composites have been evaluated using DSC and TGA. DSC thermograms revealed an increase in the melting transitions thus revealing effective fiber/matrix interface. The thermal stability in the biocomposites also increased in case of banana fiber treated with Si69. Viscoelastic measurements using DMA confirmed an increase of storage modulus and low damping values in the silane treated biocomposites. Biodegradation studies in the biocomposites have been investigated in B. cepacia medium through morphological and weight loss studies. POLYM. COMPOS., 2011. © 2011 Society of Plastics Engineers
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.