Abstract
AbstractThe microstructure and the tensile and stress-rupture properties of the nickel-base superalloy M A R-M002 have been studied using material of normal commercial composition and three melts with additions of 0·0024 and 0·0050%N and of 0·16%Si. Increasing the nitrogen content resulted in a change in carbide morphology, from ‘Chinese script’ to a blocky form, and to increased microporosity. Interference-film microscopy revealed characteristic centres in some of the blocky carbides that had high Ti contents consistent with carbide nucleation on Ti(C, N) particles formed in the melt. The increased nitrogen content was associated with a significant decrease in the rupture life at 760°C and 695 MN m−2, and a change in the fracture morphology. In the Si-doped alloy, which contained little microporosity, there were increased amounts of a phase rich in Ni–Hf (probably Ni5Hf) that also contained Si, but there was only a slight decrease in stress-rupture properties.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.