Abstract

Nano Silicon Carbide (SiC) particles have been produced by ball milling process. The sample was taken 0, 10, 20, 30, 40 and 50 hours of milling. The resulting nanoparticle powders were characterized by X-ray diffraction measurements. The high-energy ball milling of SiC after 50 hours resulted in particle size of about 24 nm. The Debye temperature, mean-square amplitudes of vibration, Debye-Waller factor, particle size, and lattice strain and vacancy formation of energies of SiC nanoparticles prepared by ball mill have been obtained from X-ray integrated intensities. The integrated intensities have been measured with a Philips CWU 3710 X-ray powder diffractometer fitted with a scintillation counter using filtered CuKα radiation at room temperature and have been corrected for thermal diffuse scattering. The X-ray Debye temperatures obtained in the present investigation has been used to estimate the vacancy formation energies for SiC nanoparticles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.