Abstract

Double layer (DL) ZnO/ZnO:Ag has been synthesized with variations in molarity of 0.1, 0.3, 0.5, and 0.7 M and its application as a degrading agent for methanil yellow dye. This study aims to determine the effect of the molarity of the DL ZnO/ZnO:Ag on crystallinity and photocatalytic activity for methanil yellow degradation. DL ZnO/ZnO:Ag was synthesized using sol-gel technique and deposited with spray coating technique. The results of DL ZnO/ZnO:Ag were characterized by XRD to determine the crystallinity and particle size. The photocatalytic activity was carried out by immersing the DL ZnO/ZnO:Ag layer in 10 ppm methanil yellow solution and irradiating it with UV light for 4 hours and then tested using UV-Vis spectroscopy to get the percentage of methanil yellow degradation. The results showed that the crystallinity of the DL ZnO/ZnO:Ag for all molarity variations had a hexagonal wurtzite structure. Grains size increase as molarity increases from 0.1 to 0.5 M. However, if the concentration continues to be increased to 0.7M, the grain size decreases. Photocatalytic activity is increasing every hour, as indicated by the increasing percentage of degradation. Precursor in 0.5 M has the maximum percentage of degradation is 25.32%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.