Abstract

The ionic conductivity, super conductivity, ferroelectricity, and magnetic resistance of barium strontium cobalt ferrite (BSCF) make it a good solid cathode material. This study aims to investigate the influence of milling process and calcination temperature on the behaviour of nanocomposite cathode BSCF–samarium-doped ceria (SDC). The BSCF–SDC composite powders were mixed using two milling processes, namely, wet milling and dry milling. The composite cathode powders were mixed through wet milling by high-energy ball milling at 550 rpm for 2 hours. For dry milling, the powders were milled at 150 rpm for 30 minutes. The powders then underwent calcination at 900 °C, 950 °C, 1050 °C, and 1150 °C for 2 hours. The composite cathodes were examined on the basis of phase and microstructure through field emission scanning electron microscopy (FESEM) and X-ray diffraction (XRD), respectively. In conclusion, the selection of suitable milling process and calcination temperature is important in eliminating secondary phases in BSCF–SDC composite cathodes and in enhancing their properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.