The influence of different raw material mixtures on β-sialon (Si6−zAlzOzN8−z, 1 ⩽ z ⩽ 4) formation through mechanical activation coupled combustion synthesis (MA-CS) was investigated in low nitriding atmosphere of 1 MPa without diluent inclusions. The MA-CS performed for the first time on sialon raw materials with milling time of 18 min obtained sialons more than three times as pure as those obtained by CS of mixtures ball milled to 1 h (z = 3). The starting materials containing silicon, aluminum, and alumina (z = 4) after MA-CS had an increment of sialon amounts up to 88 mass%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.