Abstract
The Electroluminescence (EL) intensity and the spectrum of the of the PET films under different temperatures (77K, 296K, 353K) is tested, it is found that the pre-breakdown field under the low normal and high temperature of PET films is about 3.0MV/cm, 3.2MV/cm, 3.4MV/cm, respectively, and the formation of hot electron is not the main reason that cause aging and breakdown of PET films.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.