High-alloy materials such as high chromium cast iron and high speed steel have excellent wear resistance under extreme wear conditions. But they consume much expensive chromium, molybdenum, tungsten and other alloying elements too. The hypereutectic high boron alloy has good wear resistance because it contains many high hardness primary borides. But the dimension of primary borides is big. In this paper, the hypereutectic high boron alloy was prepared using sand casting method, and the primary borides were modified by different amount of K / Na modificator. The results show that the primary boride of hypereutectic high boron alloy is Fe2B. K/Na modificator has a significant influence on primary Fe2B. The best grain refinement effect of primary Fe2B is obtained when the amount of K/Na modificator is 0.3%. The refining mechanism of primary Fe2B is that K/Na modificators can not only increase the supercooling degree to improve nucleation rate but attach to the crystal face of fastest growth direction to prevent grain from growing

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.