Abstract

This study examined the effect of ice-quenching after degassing on the change in hardness of a Pd-Au-Zn alloy during porcelain firing simulations. By ice-quenching after degassing, the specimens were softened due to homogenization without the need for an additional softening heat treatment. The lowered hardness by ice-quenching after degassing was recovered greatly from the first stage of porcelain firing process by controlling the cooling rate. The increase in hardness during cooling after porcelain firing was attributed to the precipitation of the f.c.t. PdZn phase containing Au, which caused severe lattice strain in the interphase boundary between the precipitates and matrix of the f.c.c. structure. The final hardness was slightly higher in the ice-quenched specimen than in the specimen cooled at stage 0 (the most effective cooling rate for alloy hardening) after degassing. This was attributed to the more active grain interior precipitation during cooling in the ice-quenched specimen after degassing.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.