Abstract

No-fines concrete with a compressive strength in the range 7–30MPa at 28days of curing were optimized by changing the water/cement ratio from 0.41 to 0.34 and the aggregate/cement ratio from 8 to 4. Some mixtures were also repeated with the addition of a hydrophobic admixture and prepared by fully replacing the ordinary aggregate with recycled aggregate to evaluate durability effects. High susceptibility to carbonation was observed for all the no-fines mixes studied. The use of recycled aggregate increases capillary water absorption (about 50%); however, the related decrease in durability could be easily counteracted with the use of a hydrophobic admixture.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.