Creep properties of one-step and two-step annealed Zr-1Nb-0.12O cladding tubes were studied. Creep tests were carried out at 450~500 °C with the applied stress between 80MPa and 120MPa The creep rates of the two-step annealed Zr-1Nb-0.12O alloy were found to be slower than those of the one-step annealed Zr-1Nb-0.12O alloy. The creep rate decreased with increase of grain size with annealing for Zr-1Nb-0.12O at intermediate temperatures, suggesting the creep resistance can be enhanced by the grain size control. The creep life of two-step annealed Zr-1Nb-0.12O increased over the one-step annealed Zr-1Nb-0.12O by the factor of 18~20 despite the greater initial instantaneous strain.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.