Abstract
The effect of thermal treatment on the elasto-plastic transition and mechanical properties of air plasma-sprayed 8mol% Y2O3-stabilized ZrO2 (8YSZ) thermal barrier coatings was studied by nanoindentation test at ultra-low loads with a Berkovich indenter. The area contact function of the indenter was calibrated repeatedly under nano-scales, and the indenter tip radius was estimated under different indentation depths, respectively. Owing to the heterogeneous and porous microstructure, the scatter of all collected experimental data was analyzed by Weibull statistic method. It is interesting to observe that the hardness exhibits an apparent reverse indentation size effect under very small depths. The Young's modulus of 8YSZ varies with ranging from 213 to 246GPa due to the sintering effect. True hardness of 8YSZ increases from as-received 72.9GPa to a top value 79.7GPa under 100 thermal cycles, and then slightly decreases from this value to 75.5GPa under 175 thermal cycles. The pure elastic and elasto-plastic indentation curves were obtained by adjusting the indentation load magnitude. The elasto-plastic transition and resolved shear stress fields were discussed carefully from the use of energetic models and Hertzian contact theory.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.