The kinetics of batch grinding and heat treated of ulexite using different size fractions (-3350+2360, -2360+1700, -1700+1180, 1180+850, -850+600, -600+425, -425+300, -300+212 and - 212+150 micrometers was determined using a standard Bond ball mill. It was found that breakage of ulexite follows the first order behavior for all feed sizes with the correlation coefficients equal to ap- proximately 98%. The dry grinding of the single-sized fraction and heat treatment of ulexite showed that heat treatment samples were ground much faster than the original ulexite samples.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.