Abstract

ZnS and Eu2+: ZnS QDs with different doping concentrations were prepared by co-precipitation method at room temperature. It was observed that all samples form in cubic structure. The Eu2+ (0.1%): ZnS, Eu2+ (0.3%): ZnS and Eu2+ (0.5%): ZnS QDs display broad photoluminescence emission peaks at 513.5 nm, 511. 7 nm and 510.6 nm, respectively, are related to the Eu2+ intra-ion transition of 4f6d1 – 4f7. The M-H measurements indicated that unlike ZnS QDs, Eu2+: ZnS QDs with different doping concentrations indicates ferromagnetic behavior at room temperature. The incident photon to electron conversion efficiency (IPCE) is improved with the Eu2+ doping, which proposes the QD solar cell efficiency is able to be boosted by Eu2+ doping by reason of broadened absorption spectra. Accordingly, the data point out that Eu2+: ZnS QDs with different doping concentrations are able to be appropriate materials for photovoltaic and spintronic applications.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.