Abstract

The oxidative kinetics of U-2 wt%Nb alloy with pearlitic structure at different stages (parabolic stage, transition stage, linear stage and decline stage) was uncovered using the oxygen-consumption and the reflectance spectroscopy method. Compared with U, the diffusive niobium enhances oxidative corrosion resistance of U-2 Nb at initial period. Unlike general cognition, the effect of niobium decreases with oxidative corrosion aggravating after initial period. It may result from mismatch of Nb-rich and Nb-deficient structure. The mechanism proposed in this work is propitious to the design of U-Nb binary alloys to improve their anti-corrosion property.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.